BN - Boron Nitride

Piezoelectric, Thermoelectic and Magnetic Properties


Piezoelectric constant

Zinc Blende crystal structure
e14 -0.64 C m-2 Shimada et al.(1998)
Wurtzite crystal structure
e31 0.27 C m-2 Shimada et al.(1998)
e33 -0.85 C m-2