GaInAsP - Gallium Indium Arsenide Phosphide

Piezoelectric, Thermoelectic and Magnetic Properties


Piezoelectric constant


  Remarks Referens
Piezoelectric constant e14= -(0.045+0.115x) C/m2 300 K Goldberg Yu.A. & N.M. Schmidt (1999)