| Bulk modulus | 8.8·1011 dyn cm-2 |
| Melting point | 1457 °C |
| Specific heat | 0.43 J g-1°C-1 |
| Thermal conductivity | 1.1 W cm-1 °C-1 |
| Thermal diffusivity | 0.62 cm2s-1 |
| Thermal expansion, linear | 4.65·10-6°C-1 |
![]() |
Temperature dependence of thermal conductivity. (Muzhdaba et al. [1968]). |
![]() |
Temperature dependence of specific heat. (Sirota and Sidorov [1988]). |
![]() |
Temperature dependence of linear expansion coefficient α. (Deus et al. [1983]). |
![]() |
Temperature dependence of equilibrium pressure of P2along the liquidus curve. (Ilegems et al. [1974]). |