InN - Indium Nitride

Recombination Parameters

    Remarks Referens
Radiative recombination coefficient 2.0 x 10-10 cm3 s-1. 300 K Zhou et al. (1995)
Only calculated data are available
InN. Radiative recombination coefficient B versus temperature.
Dmitriev & Oruzheinikov (1996)