Hg1Cd0Te

Number of critical points - 3

First critical point
E
1 = 2.147+0.44x+0.7x2

Second critical point:
E
1+D1 = 2.778+0.47x+0.6x2

Third critical point
E
2 = 4.8+0.66x-0.06x2

nk.gif

DATA

H.Arwin, D.E.Aspnes J.Vac.Sci.Technol. A2, 1316(1984)

L.Vina, C.Umbach, M.Cardona, and L.Vodopyanov Phys.Rev. B29, 6752(1984)